LPE removal at AECC

Hydron Industrial in collaborration with RPR Technologies demonstrating the removal of 3 Layer Poly-Ethylene and fusion bonded epoxy coating from steel piping.

The RPR 1650 utilises Induction technology to debond the coating from the steel. The middle section of the pipe had been stripped using conventional methods for demonstration purposes (manual grinding for 60-90 minutes).

The same area utilising RPR takes 15-30 minutes and leaves a surface profile ready for immediate recoating.